MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Carbon-Core CarbonMat C Polyester Laminate
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: WR330
CSM225Cm 2.0 mm
VL40
Cm 2.0 mm
CSM 300
WR 330
CSM: Chopped Strained Mat
Cm: Carbon Mat
VL: Glasstissue
WR: Wover Roving

CarbonMat non-woven polyester laminate bulker material features outstanding properties at an amazingly competitive price.

Ease of use:

  • Constant thickness
  • Deformability
  • Anti-shrinkage
  • Low resin consumption
  • Permanent bulk
  • Print-through blocking
  • Excellent fatigue resistance
  • Cost and labor effectiveness

Information provided by Carbon-Core

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Water Absorption 0.132 %0.132 %DIN 53495
Thickness 6300 microns248 mil
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 45.3 MPa6570 psilengthwise; EN 61
 65.3 MPa9470 psicrosswise; EN 61
Flexural Strength 214 MPa31000 psiEN63
Flexural Modulus 10.12 GPa1468 ksi
 
Descriptive Properties
Reinabsorption4765 g/m2
Spec weight976 g/m2DIN 53479

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCARBC016 / 190835

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.