Solid solution-strengthened developed as a filler metal for welding of dissimilar alloys. Applications include excellent dissimilar welding characteristics in the gas turbine, aerospace, and chemical process industries. Data provided by the manufacturer, Haynes International, Inc. |
AWS A5.14, ASME SFA 5.11, ASME SFA 5.14, AMS 5755, AMS 5786, AMS 5787, AWS A5.11 |