TRIEL® resins offer superior mechanical properties, elasticities, heat and chemical resistance, which allow it to be widely used for electric/electronic equipments, automotive parts and outdoor recreation equipments. TRIEL® can be processed by a variety of thermoplastic processing techniques like injection molding, extrusion and extrusion blow molding.Grade Characteristics:- Adhesive Strength
- Low Hardness
Applications: All information provided by Samyang |