MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Cast Stainless Steel E3N, ASTM A757
Categories: Metal; Ferrous Metal; Stainless Steel; Cast Stainless Steel

Material Notes: Martensitic, Corrosion Resistant, Normalized/Tempered

Key Words: ASTM A757/A757M(00), C3N
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate >= 760 MPa>= 110000 psi
Tensile Strength, Yield >= 550 MPa>= 79800 psi
Elongation at Break >= 15 %>= 15 %
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.060 %<= 0.060 %
Chromium, Cr 11.5 - 14 %11.5 - 14 %
Copper, Cu <= 0.50 %<= 0.50 %
Iron, Fe 77.8 - 84.6 %77.8 - 84.6 %As remainder
Manganese, Mn <= 1.0 %<= 1.0 %
Molybdenum, Mo 0.40 - 1.0 %0.40 - 1.0 %
Nickel, Ni 3.5 - 4.5 %3.5 - 4.5 %
Phosphorus, P <= 0.030 %<= 0.030 %
Silicon, Si <= 1.0 %<= 1.0 %
Sulfur, S <= 0.030 %<= 0.030 %
Tungsten, W <= 0.10 %<= 0.10 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
MetalTek MTEK CA6NM Cast UNS J91540 Martensitic Stainless Steel
AISI 4140H Steel, normalized at 870°C
Cast Stainless Steel CD3MN, UNS J92205
Cast Stainless Steel HD, ASTM A297
MetalTek MTEK 20 Cast UNS N08007 Super Austenitic Stainless Steel

MQCE3NA020 / 13406

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.