MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Rogers Corporation 3001 Thermoplastic Chloro-Fluorocopolymer Bonding Film
Categories: Polymer; Thermoplastic; Fluoropolymer

Material Notes: Rogers 3001 bonding film is a thermoplastic chloro-fluorocopolymer. It is recommended for bonding low dielectric constant PTFE (Teflon® fluorocarbon polymer) microwave stripline packages and other multilayer circuits. It may also be used to bond other structural and electrical components to the dielectric.
3001 bonding film features a low dielectric constant and low loss tangent at microwave frequencies, ensuring minimum interference with the electrical function of bonded stripline and other multilayer constructions.

Information provided by Rogers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Water Absorption 0.050 %
@Time 86400 sec
ASTM D570
Thickness 1.50 mil
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 115 %ASTM D882
Film Elongation at Break, TD 200 %ASTM D882
Tensile Modulus 140 ksiMD; ASTM D882
 150 ksiTD; ASTM D882
Adhesive Bond Strength 1400 psiRogers Test Method
Film Tensile Strength at Break, MD 7500 psiASTM D882
Film Tensile Strength at Break, TD 5500 psiASTM D882
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+17 ohm-cmASTM D257
Surface Resistance 1.00e+15 ohmASTM D257
Dielectric Constant 2.28Z direction, X-Band; Two stacks of 40 piles of film are used; IPC-TM-650 2.5.5.5
Dielectric Strength 2500 V/milZ Direction; ASTM D149
Dissipation Factor 0.0030Z direction; X-band; IPC-TM-650 2.5.5.5
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.220 W/m-KZ direction
Melting Point 186 °CCrystalline
Maximum Service Temperature, Air 176 °C
 
Descriptive Properties
Tensile, CMD (lb) per ASTM D8825500ASTM D882
Tensile, MD (lb) per ASTM D8827500ASTM D882

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Rogers Arlon CuClad 6700 Bonding Film
Rogers Arlon CuClad 6250 Bonding Film
Rogers Arlon CLTE-P Pre-Preg Bonding Layer
Honeywell UltRx 400 CTFE Homopolymer, Barrier Film
Honeywell ACLAR® UltRx 3000 CTFE Homopolymer, Barrier Film

PROGA969 / 138409

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.