MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Morgan Advanced Ceramics Firemaster Board 550 Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: Alkaline Earth Silicate. Made exclusively from low bio-persistent alkaline earth silicate (AES) fibres, refractory fillers and selected binders, this board is recommended for fire protection of structural elements where high strength and good machinable properties are required. FireMaster® 550 board is available in large panel sizes and has good screw holding strength making it ideal for the construction of walls, ceilings and partition systems. FireMaster® 550 board has advantages of lower weight and lower thermal conductivity than calcium silicate boards together with the benefit of water repellence. In addition, ireMaster® 550 board has low dust emission during cutting operations.

Applications:

  • Structural steel fire protection (FireMaster® 550 board)
  • Fire damper systems insulation (FireMaster® 550 board)
  • Core material for fire rated decorative veneered panel systems
  • Ducting system

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.550 g/cc
Absorption Coefficient 0.14
@Frequency 125 Hz
test to BS EN 20354: 1993 Method
 0.15
@Frequency 1000 Hz
test to BS EN 20354: 1993 Method
 0.18
@Frequency 2000 Hz
test to BS EN 20354: 1993 Method
 0.19
@Frequency 500 Hz
test to BS EN 20354: 1993 Method
 0.21
@Frequency 4000 Hz
test to BS EN 20354: 1993 Method
 0.23
@Frequency 250 Hz
test to BS EN 20354: 1993 Method
 
Mechanical PropertiesOriginal ValueComments
Modulus of Rupture 0.00300 GPa
Compressive Strength 1.10 MPa10% reduction in thickness
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.110 W/m-K
@Temperature 200 °C
ASTM C-201-68
 0.120 W/m-K
@Temperature 300 °C
ASTM C-201-68
 0.130 W/m-K
@Temperature 400 °C
ASTM C-201-68
 0.140 W/m-K
@Temperature 500 °C
ASTM C-201-68
 
Descriptive Properties
Colortan
Noise Reduction Coefficient0.19
Screw Holding Strength (kg)1313mm penetration depth, board to BS 3535: Part 2: 1974
 2018mm penetration depth, board to BS 3535: Part 2: 1974
Specific Strength Test Max. Deflection (mm)1.23Load bearing for 40mm, 1200mmx600mm board sample with 2mm steel plate facing, Uniformly applied load, 350kg load
 1.52Load bearing for 40mm, 1200mmx600mm board sample with 2mm steel plate facing, Uniformly applied load, 500kg load
 1.56Load bearing for 40mm, 1200mmx600mm board sample with 2mm steel plate facing, edge applied load on plate 80mmx80mm, 115kg load
 1.66Load bearing for 40mm, 1200mmx600mm board sample with 2mm steel plate facing, Edge applied load on plate 80mmx80mm, 165kg load
 1.9Load bearing for 40mm, 1200mmx600mm board sample with 2mm steel plate facing, centrally applied load on plate 80mmx80mm, 115kg load
 2.02Load bearing for 40mm, 1200mmx600mm board sample with 2mm steel plate facing, centrally applied load on plate 80mmx80mm, 165kg load

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BNZ Materials Transite HT Low Temperature Industrial Board
BNZ Materials Transite 1000 Low Temperature Industrial Board
Pyrotek ISOMAG® 45 Thermal Insulation Board
Pyrotek B-3A REFRACTORY BOARD
Morgan Advanced Ceramics Kaowool® Cement B

CMORF6072 / 202856

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.