MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Hapco DI-COAT™ R-4721/30 Coating
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: Shore 90 D, room temperature curing, medium to high thixotropic coating for dielectric insulating applications. DI-COAT™ R-4721 is ideal for use on vertical or sloping surfaces where flow or drain-off cannot be tolerated. DI-COAT™ R-4721 is easy to use, and should be used on insulating applications where conformal coating is required. DI-COAT R-4721 LV exhibits similar characteristics to DI-COAT R-4721, but has a lower viscosity.

Information provided by Hapco, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.50 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 90
Tensile Strength 8700 psi
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.96e+12 ohm-cm
Dielectric Constant 3.0
@Frequency 100000 Hz
ASTM D-150
 3.1
@Frequency 1000 Hz
ASTM D-150
Dielectric Strength 600 V/mil
Dissipation Factor 0.024
@Frequency 100000 Hz
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Inert 175 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 4.00 - 6.00 hour
@Temperature 48.9 °C
Plus 6-12 hours @ 200ºF
Gel Time 100 - 140 min
 
Descriptive Properties
Color (cured)White
Mix Ratio100A:13BWeight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHAPCO054 / 317113

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.