MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

HB Fuller AT-1 Very High Bond Strength Acrylic Tape
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: AT-1 is a pressure sensitive, water-clear, solid acrylic tape system designed to provide a superior bond between a wide variety of substrates. The tape possesses a uniform, high-tack, acrylic adhesive on both surfaces and will bond to most clean, dry, oil-free substrates. Thickness ranges from 0.25mm to 1.5mm (0.010” to 0.060”) Width ranges from 6mm to 457mm (0.25” to 18”)

Features and Benefits: AT-1 offers numerous advantages including a waterproof bond, ease of application, and the ability to withstand thermal movement.

  • Transparent appearance works well with applications involving glass or other clear materials
  • Pressure sensitive bonding
  • Solid composition for easy cutting
  • Moisture resistant
  • Excellent weathering properties
  • Maintains adhesion at sub-zero temperatures
  • Hardening or brittle resistant with age
  • Flexible – conforms to intricate shapes
Typical Applications:
  • Auto trim attachment
  • Signs
  • Graphics
  • Skin to frame assembly
  • Furniture
  • Appliances
  • Many other manufacturing and construction applications to replace mechanical fasteners and welds

Information provided by H.B. Fuller Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Storage Temperature 4.00 - 38.0 °C39.2 - 100 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 1.70 MPa247 psiASTM D412 Die C
Elongation at Break 1000 %1000 %ASTM D412 Die C
Shear Strength 0.415 MPa60.2 psiDynamic; ASTM D3163
Peel Strength 4.40 kN/m25.1 pli90° Peel Adhesion; ASTM D3330
 10.4 kN/m59.3 pliCleavage Peel, Diesel Fuel - 1hr; FLTM BU 112-02, Method C
 11.4 kN/m65.0 pliCleavage Peel, Water Immersion - 240hrs; FLTM BU 112-02, Method C
 11.4 kN/m65.0 pliCleavage Peel, Unleaded Gasoline - 1hr; FLTM BU 112-02, Method C
 12.3 kN/m70.2 pliCleavage Peel, 3 Days @ RT; FLTM BU 112-02, Method C
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 93.0 °C199 °F
Minimum Service Temperature, Air -34.0 °C-29.2 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 24.0 Month24.0 Month
 
Descriptive Properties
ColorWater-clear

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHBFULL114 / 316905

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.