MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Hexcel® HexWeb® CRF-3/8-ACG-.002-2.3 Chromate free ACG® Honeycomb  (discontinued **)
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 3000 Series Aluminum Alloy

Material Notes: Hexweb CRF is a hexagonal cell aluminum honeycomb material used principally as a shear carrying core in light weight adhesively bonded sandwich structures, and suitable for a wide range of other applications.
Hexweb CRF is available in a number of cell sizes and densities allowing versatility in design of sandwich structures with minimum weight but maximum stiffness and bucking resistance.
Hexweb CRF utilizes the benefits of a chromate free corrosion protection coating.

Key Features: Chromate free corrosion protection coating; Good strength and stiffness to weight ratio; High fatigue resistance; Good vibration damping characteristics; Non-combustible; Can be machined to complex profiles; Exhibits uniform crushing characteristics; Compatible with a wide range of skin materials, providing a good bonding surface for Redux® adhesives.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Compressive Yield Strength 1.40 MPaStabilized
Compressive Modulus 0.240 GPa
Shear Modulus 0.0900 GPaPlate Shear, W direction
 0.190 GPaPlate Shear, L direction
Shear Strength 0.450 MPaPlate Shear, W direction
 0.800 MPaPlate Shear, L direction

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Stainless Steel
Overview of materials for 6000 Series Aluminum Alloy
Overview of materials for 3000 Series Aluminum Alloy
Hexcel® HexWeb® CRF-1/4-ACG-.003-15.2 Chromate free ACG® Honeycomb
Hexcel® HexWeb® ACG®-1/4 Honeycomb Aluminum Commercial Grade

PHEXC311 / 98782

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.