MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Suqian Unitechem Antioxidant 3114
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Chemical Name: Tris(3,5-di-tert-butyl-4-hydroxybenzyl) isocyanurate

CAS NO.: 27676-62-6

Molecular Formula: C48H69N3O6

Property: It is one kind of multi-functional Antioxidant, with multiple functional groups. It is one kind of low toxic chemicals, and it can be used in food packing.

Uses: It can be used in ABS resin, polyester, Nylon, PE, PS, PVC, PU, cellulose plastic and rubber. It can work with UV absorbent or phosphite ester to improve the stability.

Dosage: 0.1-0.25%.

Information Provided by Suqian Unitechem Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density <= 1.03 g/cc<= 0.0372 lb/in³Relative density
Volatiles <= 0.20 %<= 0.20 %
Molecular Weight 784.1 g/mol784.1 g/mol
Ash <= 0.10 %<= 0.10 %
 
Thermal PropertiesMetricEnglishComments
Melting Point 218 - 223 °C424 - 433 °F
Flash Point 289.4 °C552.9 °F
 
Optical PropertiesMetricEnglishComments
Transmission, Visible >= 93 %>= 93 %425nm
 >= 95 %>= 95 %500nm
 
Descriptive Properties
AppearanceWhite powder
Purity (%)>98

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI 1045 Steel, cold drawn, 19-32 mm (0.75-1.25 in) round
Overview of materials for Low Alloy Steel

PSUQI10 / 103993

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.