MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Ravago Manufacturing Americas Ravatuf™ 400X2 Polyolefin
Categories: Polymer; Thermoplastic; Polyolefin

Material Notes: Product Description: An engineered TPO with high stiffness and good impact intended for molding applications. This grade offers excellent dimensional stability, low shrinkage, UV stability and good chemical resistance.
Features: Molding grade with good dimensional stability and low shrinkage; Ease of coloring by using PE or PP based color concentrates; Ease of processing; Recyclability

Availability: North America

Features: Chemical Resistant; Good Colorability; Good Impact Resistance; Good Processability; High Dimensional Stability; High Stiffness; Low Shrinkage; Recyclable Material; UV Resistant

Processing Method: Injection Molding

Information provided by Ravago Manufacturing Americas

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.15 g/ccASTM D792
Melt Flow 30 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 2900 psiASTM D638
Flexural Modulus 363000 psi1% Tangent, 0.05 min/min; ASTM D790
Izod Impact, Notched 25.0 ft-lb/inASTM D256
Gardner Impact 374 in-lbASTM D5420
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 46.0 µin/in-°FASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 329 °FUnannealed; ASTM D648
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 375 - 410 °F
Middle Barrel Temperature 392 - 430 °F
Front Barrel Temperature 410 - 445 °F
Nozzle Temperature 410 - 445 °F
Melt Temperature 410 - 445 °F
Mold Temperature 50.0 - 122 °F
Drying Temperature 160 - 190 °F
Dry Time 2.00 - 3.00 hour
Screw Speed 50 - 200 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PRAVAGO41249 / 311942

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.