MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Sulfur, S, Alpha (Room Temperature Form)
Categories: Pure Element

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.07 g/cc0.0748 lb/in³
 
Chemical PropertiesMetricEnglishComments
Atomic Mass 32.06632.0661995
Atomic Number 1616
X-ray Absorption Edge 5.0182 Å5.0182 ÅK
 64.228 Å64.228 ÅLI
 76.049 Å76.049 ÅLII
 76.519 Å76.519 ÅLIII
Critical Temperature 1041 °C1906 °F
Electronegativity 2.582.58Pauling
Ionic Radius 0.300 Å0.300 ÅCrystal Ionic Radius for Valence +6
 0.370 Å0.370 ÅCrystal Ionic Radius for Valence +4
 1.84 Å1.84 ÅCrystal Ionic Radius for Valence -2
 2.19 Å2.19 ÅCrystal Ionic Radius for Valence +2
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 0.710 J/g-°C0.170 BTU/lb-°F
Boiling Point 444.6 °C832.3 °F
Transformation Temperature 95.3 °C204 °FTransforms to Beta Form
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.917
@Temperature 125 °C,
Wavelength 589 nm
1.917
@Temperature 257 °F,
Wavelength 589 nm
 
Component Elements PropertiesMetricEnglishComments
Sulfur, S 100 %100 %
 
Descriptive Properties
AppearanceYellow Orthogonal Crystals
CAS Number7704-34-9
 7704-34-9

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Crucible Steel CPM® Rex® 76®(HS), AISI M48 High Speed Steel Rex® 76®(HS)
Phosphorous, P, White
AISI 1021 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
Graphite, Carbon, C
Nitrogen, N2

AMES / 3915

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.