MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Eifeler Coatings Technology VARIANTIC® TiAlCN PVD Coating
Categories: Ceramic; Nitride; Other Engineering Material; Ceramic/Metallic Coating

Material Notes: Key Characteristics: low friction, good oxidation resistance

Primary Applications: coating for a wide range of carbide, cermet and high speed steel tools; machining of all types of steel under dry as well as wet machining conditions; drawing, stamping, punching, forming tools for processing of high and low alloy steel, orthopedic instrumentation

Information provided by Eifeler Coatings Technology

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 2.00 - 4.00 microns0.0787 - 0.157 mil
 
Mechanical PropertiesMetricEnglishComments
Vickers Microhardness 3000 - 40003000 - 4000
Coefficient of Friction 0.200.20dry, steel
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 800 °C1470 °F
 
Descriptive Properties
Colorold rose

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
SMAC SMACTANE® SP Damping Material
SMAC SMACTANE® 70 1114S- N04 Damping Material
SMAC SMACSONIC® Carbon EX Noise and Vibration Damping
SMAC SMACSIL® 1114S- S02 Damping Material
Parker Chomerics T-Wings Heat Spreaders

NEIFEL014 / 175969

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.