OROGLAS MI-4T is an acrylic grade that associates improved impact resistance with high heat resistance. Key features - improved impact resistance: up to 4 times more impact resistant than standard acrylics.
- outstanding thermal resistance: HDT A (1.82 MPa) = 98°c.
- good flow and processing behavior.
- UV stability.
- clarity, brilliance and excellent optical properties.
Typical applications OROGLAS MI-4T can be injection molded or extruded to produce technical items mainly for automotive and lighting markets. ISO data provided by the manufacturer, Arkema. |