MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Geon® Performance Solutions Vinyl Wire & Cable JAC31L PVC, Flexible  (discontinued **)
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Flexible Grade; PVC, Wire and Cable Grade

Material Notes: Typical Properties of Molded Slab (0.075"); Not to be Construed as Specifications.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.41 g/cc1.41 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 49
@Time 15.0 sec
49
@Time 0.00417 hour
ASTM D2240
Tensile Strength at Break 20.7 MPa3000 psiType IV, 510 mm/min; ASTM D638
Elongation at Break 280 %280 %Type IV, 510 mm/min; ASTM D638
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmASTM D257
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 90.0 °C194 °FUL Temperature Rating
Brittleness Temperature -28.0 °C-18.4 °FASTM D746
Oxygen Index 34 %
@Thickness 1.91 mm
34 %
@Thickness 0.0752 in
ASTM D2863
 
Processing PropertiesMetricEnglishComments
Melt Temperature 177 - 182 °C351 - 360 °F
 
Descriptive Properties
Agency RatingsUL 444
FeaturesFlame Retardant
FormsPellets
Processing MethodExtrusion Coating
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
Retention of Elongation, %80336 hr, UL Standard; 121°C, 1.91 mm
Retention of Tensile Strength, %100336 hr, UL Standard; 121°C, 1.91 mm
RoHS ComplianceRoHS Compliant
UsesCommunication Wire Jacketing
 Wire & Cable Applications
Wire TypesCL2
 CL2R
 CL3R
 CMR
 FPLR

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M Dyneon™ PVDF 11008/0003 Polyvinylidene Fluoride
BASF Ultradur® B 6550 LN PBT
BASF Ultradur® B 6550 L PBT
Arkema Kynar Flex® 3030-15 PVDF
LyondellBasell Pro-fax 6323 Polypropylene Homopolymer, Easy Molding

PH1PN8913 / 102749

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.