MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Johnson Matthey Copper-flo™ Copper-Phosphorus Brazing Filler Metal
Categories: Metal; Nonferrous Metal; Copper Alloy; Solder/Braze Alloy

Material Notes: Copper-flo™ is a copper-phosphorus brazing filler metal containing a nominal 7.8% phosphorus. It is primarily used for the brazing of copper, although it can also be used for brazing copper alloys. When brazing copper the phosphorus within the alloy imparts a metallurgical based self-fluxing capability. Copper-flo™ does not contain a flux core or flux coating. If used to join copper alloys (such as brass, bronze or gun metal) a separate flux will be required because the self-fluxing action only occurs on copper.

This filler metal should not be used to braze iron containing materials like carbon or stainless steels or nickel containing materials as the phosphorus within the filler metal will form brittle, intermetallic, phosphide compounds at the joint interface. Copper-flo™ is not suitable for use in sulfurous atmospheres at elevated service temperatures.

When selecting a copper-phosphorus brazing filler metal it is necessary to understand about their flow properties and ductility. The level of phosphorus within the filler metal controls these two characteristics - the higher this is the more free flowing the filler metal and the lower its ductility.

Copper-flo™ is the most free flowing copper-phosphorus filler metal. However, due to its high phosphorus content it is one of the least ductile. The low ductility of the alloy imparts it with glass like properties, making it both ‘notch’ sensitive and sensitive to impact type loadings. This filler metal should therefore not be used in applications involving exposure to strong vibration, impact loads or where some deformation of the joint might be expected in service.

Copper-flo™ is best suited for making copper joints that are of the true capillary type and where tight joint clearances of 0.025-0.075 mm are used. The use of ‘bell mouthed’ type joints should be avoided. Copper-flo™ can be used to braze copper alloys, but its lack of ductility can be exposed in such applications.

Copper-flo™ is widely used in the refrigeration, heating and ventilating and air conditioning industries for the brazing of copper pipe-work systems.

Information provided by Johnson Matthey Metal Joining

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesMetricEnglishComments
Melting Point 714 - 770 °C1320 - 1420 °F
Solidus 714 °C1320 °F
Liquidus 770 °C1420 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 92.2 %92.2 %
Phosphorus, P 7.8 %7.8 %
 
Descriptive Properties
Approximate Flow Point720°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Eagle Brass 19210 XP-10 Copper Iron, Annealed
Eagle Brass 19210 XP-10 Copper Iron, Hard
Copper, UNS C19210, H01 Temper sheet
Overview of materials for Solder/Braze Alloy
PSM Industries Pacific Sintered Metals FC-203-N Copper Iron Powdered Metal (MPIF FC-1000-20)

NJMMJ9727 / 186128

solder replacement adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.