MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Total 4620WZ Polypropylene, Impact Copolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: ATOFINA 4620WZ polypropylene is a nucleated impact copolymer, combining good fluidity and mechanical properties. 4620WZ is characterized by improved stiffness, creep resistance, high impact resistance, excellent antistatic properties and is formulated to allow faster cycling through early demolding.

Application

ATOFINA 4620WZ has been developed specifically for the injection molding of buckets, pails, toys, housewares and garden furniture.

Information provided provided by Total Petrochemicals.

Total Petrochemicals includes former Fina and Atofina plastics product lines.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.905 g/cc0.0327 lb/in³ASTM D1505
Melt Flow 13 g/10 min13 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 28.3 MPa4100 psiASTM D638
Elongation at Yield 6.0 %6.0 %ASTM D638
Flexural Modulus 1.52 GPa220 ksiASTM D 790
Izod Impact, Notched 1.05 J/cm1.97 ft-lb/inASTM D256
 0.450 J/cm
@Temperature -20.0 °C
0.843 ft-lb/in
@Temperature -4.00 °F
ASTM D256
Charpy Impact Unnotched 1.10 J/cm²5.24 ft-lb/in²Notched/Unnotched not specified; ASTM DIN53453
 0.500 J/cm²
@Temperature -20.0 °C
2.38 ft-lb/in²
@Temperature -4.00 °F
Notched/Unnotched not specified; ASTM DIN53453
 
Thermal PropertiesMetricEnglishComments
Melting Point 160 - 165 °C320 - 329 °FATOFINA Method
Deflection Temperature at 0.46 MPa (66 psi) 93.0 °C199 °FASTM D648
Vicat Softening Point 152 °C306 °FASTM D1525

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PFINAA070 / 38506

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.