MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Colour Image Plastic Compound Toughblend® PA66-1600 Nylon 66, 30% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: Product Description: Toughblend® PA66-1600 is a glass fiber reinforced compound characterized by excellent thermal and mechanical properties.

Features:

  • Glass Fiber Reinforcement, 30%
  • Excellent thermal & mechanical properties
Uses:
  • Automotive Applications
  • Industrial parts
Forms:
  • Pellets
Processing Method:
  • Injection Molding

Information provided by Colour Image Plastic Compound Sdn Bhd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.37 g/cc1.37 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
0.0050 - 0.0070 in/in
@Thickness 0.126 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 190 MPa27600 psiASTM D638
Elongation at Break 2.5 %2.5 %ASTM D638
Flexural Strength 275 MPa39900 psiASTM D790
Flexural Modulus 9.25 GPa1340 ksiASTM D790
Izod Impact, Notched 1.20 J/cm2.25 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 260 °C
@Thickness 4.00 mm
500 °F
@Thickness 0.157 in
Unannealed; ASTM D648
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 275 - 280 °C527 - 536 °F
Middle Barrel Temperature 280 - 285 °C536 - 545 °F
Front Barrel Temperature 285 - 290 °C545 - 554 °F
Nozzle Temperature 290 - 295 °C554 - 563 °F
Melt Temperature 275 - 295 °C527 - 563 °F
Mold Temperature 70.0 - 100 °C158 - 212 °F
Drying Temperature 90.0 °C194 °F
Dry Time 4.00 hour4.00 hour
 <= 8.00 hour<= 8.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCOLO006 / 265898

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.