MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Chase Plastics CP Pryme® NN113L (Dry) Nylon 66, 13% Glass Fiber Reinforced, Lubricated
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 10% Glass Fiber Filled

Material Notes: Features:
  • Good chemical resistance
  • Grease resistant
  • Lubricated
  • Oil resistant
  • High rigidity
  • Solvent resistant
  • High tensile strength

Form: Pellets

Information provided by Chase Plastics.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.22 g/cc0.0441 lb/in³ASTM D792
Filler Content 13 %13 %
Water Absorption 1.0 %1.0 %At 24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.0040 - 0.0080 cm/cm0.0040 - 0.0080 in/in0.125 in; ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 9595ASTM D785
Tensile Strength at Break 124 MPa18000 psiASTM D638
Elongation at Break 3.0 %3.0 %ASTM D638
Flexural Strength 179 MPa26000 psiASTM D790
Flexural Modulus 5.52 GPa800 ksiASTM D790
Izod Impact, Notched 0.801 J/cm1.50 ft-lb/in0.125 in; ASTM D256
 
Thermal PropertiesMetricEnglishComments
Melting Point 260 °C500 °F
Deflection Temperature at 1.8 MPa (264 psi) 245 °C473 °FUnannealed; ASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman SCHULAMID® 66 GF13 13% Glass Fiber Reinforced Nylon 66
Teknor Apex Chemlon 102 Nylon 66, Nucleated
Adell AR-13 Nylon 66, 15% Glass Reinforced
A. Schulman Diamond NYLON 6615 HS Natural
Asahi Kasei Leona™ FG170 Polyamide 66, GF Reinforced, Flame Retardant

PCHA031 / 28027

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.