MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Akrochem Cure-Rite® 18 Powder
Categories: Other Engineering Material

Material Notes: Product Description: Cure-Rite® 18 is a non-staining, primary accelerator for natural and synthetic rubbers such as EPDM, SBR, Nitrile and Butyl. Cure-Rite® 18 is more efficient than other sulfenamide accelerators. As a result, a 25% reduction in the sulfenamide portion of an accelerator system is possible when Cure- Rite® 18 is used. This substitution will result in no loss of cure rate while maintaining good physical properties.

Application: Cure-Rite® 18 can be utilized to produce excellent economical, semi-EV cure systems. The preferred dosage ratio is 2 parts Cure-Rite® 18 to 1 part of another sulfenamide like BBTS or CBTS. Sulfur loading should be kept low, 0.4 to 0.6 PHR. Thiazoles may be used in place of the sulfenamides to speed up the cure rate and reduce reversion in natural rubber. Heat aging and compression set properties are outstanding. Processing properties are excellent, providing fast cure rates with good scorch safety. Accelerator Cure-Rite® 18 is also available as a polymer bound dispersion (Akrochex® OTOS-70/EPR/C-LB). Polymer bound or encapsulated dispersions are a proven means of upgrading plant safety, efficiency, quality and raw material control.

Information provided by Akrochem Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.35 g/cc
Ash <= 0.50 %
 
Thermal PropertiesOriginal ValueComments
Melting Point >= 133 °C
 
Descriptive Properties
Appearancewhite powder
Heat Loss<0.2%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PAKZCH446 / 315364

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.