MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Overview of materials for AISI 1000 Series Steel
Categories: Metal; Ferrous Metal; Carbon Steel; AISI 1000 Series Steel

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "AISI 1000 Series Steel". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.80 - 7.87 g/ccAverage value: 7.86 g/cc Grade Count:604
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 30.0 - 500Average value: 190 Grade Count:577
Hardness, Knoop 103 - 392Average value: 210 Grade Count:513
Hardness, Rockwell B 49.0 - 100Average value: 86.3 Grade Count:511
Hardness, Rockwell C 9.00 - 71.0Average value: 19.1 Grade Count:267
Hardness, Vickers 88.0 - 384Average value: 197 Grade Count:513
Tensile Strength, Ultimate 295 - 2210 MPaAverage value: 649 MPa Grade Count:578
Tensile Strength, Yield 165 - 1260 MPaAverage value: 450 MPa Grade Count:578
Elongation at Break 5.00 - 48.0 %Average value: 19.8 % Grade Count:572
Reduction of Area 13.4 - 72.5 %Average value: 46.8 % Grade Count:561
Modulus of Elasticity 186 - 210 GPaAverage value: 201 GPa Grade Count:592
Bulk Modulus 148 - 163 GPaAverage value: 160 GPa Grade Count:535
Poissons Ratio 0.290 - 0.300Average value: 0.290 Grade Count:592
Machinability 40.0 - 160 %Average value: 59.7 % Grade Count:143
Shear Modulus 72.0 - 80.0 GPaAverage value: 79.5 GPa Grade Count:590
Izod Impact 3.00 - 135 JAverage value: 42.8 J Grade Count:273
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000200 - 0.0000180 ohm-cmAverage value: 0.0000166 ohm-cm Grade Count:398
 
Thermal PropertiesOriginal ValueComments
CTE, linear 11.0 - 16.6 µm/m-°CAverage value: 12.9 µm/m-°C Grade Count:539
Specific Heat Capacity 0.470 - 0.490 J/g-°CAverage value: 0.472 J/g-°C Grade Count:263
Thermal Conductivity 27.1 - 52.0 W/m-KAverage value: 51.0 W/m-K Grade Count:472
Melting Point 1430 °CAverage value: 1430 °C Grade Count:3
Transformation Temperature 270 - 760 °CAverage value: 591 °C Grade Count:18
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 0.0150 - 0.0200 %Average value: 0.0170 % Grade Count:5
Carbon, C 0.0600 - 1.03 %Average value: 0.402 % Grade Count:620
Chromium, Cr 0.150 - 1.10 %Average value: 0.341 % Grade Count:24
Copper, Cu 0.250 - 0.300 %Average value: 0.275 % Grade Count:10
Iron, Fe 96.8 - 100 %Average value: 98.5 % Grade Count:620
Lead, Pb 0.150 - 0.360 %Average value: 0.251 % Grade Count:7
Manganese, Mn 0.250 - 2.05 %Average value: 0.927 % Grade Count:620
Molybdenum, Mo 0.0600 - 0.250 %Average value: 0.109 % Grade Count:17
Nickel, Ni 0.100 - 0.400 %Average value: 0.298 % Grade Count:23
Phosphorus, P 0.0200 - 0.400 %Average value: 0.0422 % Grade Count:618
Silicon, Si 0.100 - 0.400 %Average value: 0.262 % Grade Count:73
Sulfur, S 0.0150 - 0.500 %Average value: 0.0792 % Grade Count:620
Titanium, Ti 0.00500 %Average value: 0.00500 % Grade Count:3
Vanadium, V 0.0300 - 0.100 %Average value: 0.0587 % Grade Count:4

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for AISI 4000 Series Steel
Overview of materials for Low Carbon Steel
Overview of materials for Low Alloy Steel
Overview of materials for Medium Carbon Steel
AISI 1005 Steel

M01008 / 81705

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.