MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

LG Chemical ER462 Injection Molding Grade
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Molded

Material Notes: High Flow, Medium High Heat

Applications: Automotives, E&E, miscellaneous goods

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³ASTM D792
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
@Thickness 3.20 mm
0.0040 - 0.0070 in/in
@Thickness 0.126 in
ASTM D955
Melt Flow 50 g/10 min
@Load 10.0 kg,
Temperature 220 °C
50 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 43.0 MPa
@Thickness 3.20 mm
6230 psi
@Thickness 0.126 in
50 mm/min; ASTM D638
Flexural Strength 60.0 MPa
@Thickness 3.20 mm
8700 psi
@Thickness 0.126 in
15 mm/min; ASTM D790
Flexural Modulus 2.10 GPa
@Thickness 3.20 mm
304 ksi
@Thickness 0.126 in
15 mm/min; ASTM D790
Izod Impact, Notched  1.60 J/cm
@Thickness 6.40 mm
2.99 ft-lb/in
@Thickness 0.252 in
ASTM D256
 2.40 J/cm
@Thickness 3.20 mm
4.50 ft-lb/in
@Thickness 0.126 in
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C
@Thickness 6.40 mm
194 °F
@Thickness 0.252 in
Unannealed; ASTM D648
Vicat Softening Point 98.0 °C
@Load 5.10 kg
208 °F
@Load 11.2 lb
50°C/h; ASTM D1525
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 180 - 210 °C356 - 410 °F
Middle Barrel Temperature 210 - 230 °C410 - 446 °F
Front Barrel Temperature 230 - 240 °C446 - 464 °F
Nozzle Temperature 230 - 240 °C446 - 464 °F
Melt Temperature 230 - 260 °C446 - 500 °F
Mold Temperature 40.0 - 60.0 °C104 - 140 °F
Drying Temperature 80.0 °C
@Time 10800 - 14400 sec
176 °F
@Time 3.00 - 4.00 hour
Moisture Content <= 0.050 %<= 0.050 %
Back Pressure 0.981 - 2.94 MPa142 - 426 psi
Screw Speed 30 - 60 rpm30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLHCHEM9946 / 239462

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.