MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Menzolit Menzolit® BMC 0800 Unsaturated Polyester UP
Categories: Polymer; Thermoset; Polyester, TS; Thermoset Polyester Glass SMC

Material Notes: BMC 0800 is a special SMC for applications within household and kitchenware. The glass level has been selected to combine good mould ability with good strength and stiffness properties. The product shows good resistance to food chemicals, cleaning detergents, water and mechanical abrasion. Typical applications are trays and components for dishwashing and food processing machinery.

Information Provided by Menzolit

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.90 g/ccISO 1183
Water Absorption <= 0.30 %ISO 62
Linear Mold Shrinkage 0.0015 cm/cmISO 2577
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 37.0 MPa
@Temperature 22.0 °C
25 mm flat samples, compression molded; ISO 527-4
Tensile Strength, Yield 37.0 MPa
@Temperature 22.0 °C
25 mm flat samples, compression molded; ISO 527-4
Elongation at Break 0.00 %ISO 527-4
Modulus of Elasticity 13.0 GPa25 mm flat samples, compression molded; ISO 527-4
Flexural Strength 120 MPa
@Temperature 22.0 °C
25 mm wide 100 mm long, flat samples; ISO 14125
Flexural Modulus 10.0 GPa
@Temperature 22.0 °C
25 mm wide 100 mm long, flat samples; ISO 14125
Poissons Ratio 0.30
Shear Modulus 5.00 GPain plane
Charpy Impact, Notched 3.00 J/cm²ISO 179
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+12 ohmIEC 60093
Dielectric Constant 4.0IEC 60250
Dielectric Strength 30.0 kV/mmIEC 60243-1
Dissipation Factor 0.010IEC 60250
Comparative Tracking Index 600 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear 10.0 µm/m-°CISO 11359-2
Specific Heat Capacity 1.10 J/g-°C
Thermal Conductivity 0.700 W/m-K
Maximum Service Temperature, Air 140 °C
Deflection Temperature at 1.8 MPa (264 psi) >= 150 °CISO 75-2
Minimum Service Temperature, Air -40.0 °C
Glass Transition Temp, Tg 125 °CISO 11357-2
Flammability, UL94 HB
@Thickness 3.00 mm
Oxygen Index 22 %ISO 4589-2
Glow Wire Flammability Index 750 °CIEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Processing Temperature 135 - 150 °CInjection molding, matched metal die

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Menzolit Menzolit® SMC 0150 Unsaturated Polyester UP
Menzolit Menzolit® SMC 0180 Unsaturated Polyester UP
Menzolit Menzolit® SMC 0160 Unsaturated Polyester UP
Haysite 46000 Polyester SMC, 30% Glass Reinforced
Menzolit Menzolit® SMC 0600 Unsaturated Polyester UP

PMENZ010 / 100744

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.