MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
AISI 1015 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
Categories: Metal; Ferrous Metal; Carbon Steel; AISI 1000 Series Steel; Low Carbon Steel

Material Notes: This steel demonstrates better machinability and carburizing. Can be strengthened by cold working or surface hardened by carburizing or cyaniding. Hot rolled sheet has excellent weldability.

Key Words: UNS G10150, AMS 5060, ASTM A29, ASTM A108, ASTM A510, ASTM A545, ASTM A549, ASTM A575, ASTM A576, ASTM A659, FED QQ-S-698 (C1015), MIL SPEC MIL-S-16974, SAE J403, JIS S 17 C, JIS S 15 CK, SS14 1370 (Sweden), SAE J412, SAE J414, DIN 1.1141, AFNOR XC 15 (Fr), AFNOR XC 18 (Fr), JIS S 15 C, AISI1015
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.87 g/ccTypical for steel
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 101
Hardness, Knoop 119Converted from Brinell
Hardness, Rockwell B 58Converted from Brinell
Hardness, Vickers 104Converted from Brinell
Tensile Strength, Ultimate 345 MPa
Tensile Strength, Yield 190 MPa
Elongation at Break 28 %in 50 mm
Reduction of Area 50 %
Modulus of Elasticity 200 GPaTypical for steel
Bulk Modulus 160 GPaTypical for steel
Poissons Ratio 0.29Typical For Steel
Machinability 60 %Based on 100% machinability for AISI 1212 steel.
Shear Modulus 80.0 GPaTypical for steel
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000159 ohm-cm
@Temperature 0.000 °C
annealed condition
 0.0000219 ohm-cm
@Temperature 100 °C
annealed condition
 0.0000292 ohm-cm
@Temperature 200 °C
annealed condition
 
Thermal PropertiesOriginal ValueComments
CTE, linear 11.9 µm/m-°C
@Temperature 0.000 - 100 °C
 12.4 µm/m-°C
@Temperature 0.000 - 200 °C
 13.0 µm/m-°C
@Temperature 0.000 - 300 °C
 13.5 µm/m-°C
@Temperature 0.000 - 400 °C
 14.2 µm/m-°C
@Temperature 0.000 - 500 °C
Specific Heat Capacity 0.486 J/g-°C
@Temperature >=100 °C
annealed
Thermal Conductivity 51.9 W/m-Kestimated based on similar materials
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.13 - 0.18 %
Iron, Fe 99.13 - 99.57 %As remainder
Manganese, Mn 0.30 - 0.60 %
Phosphorus, P <= 0.040 %
Sulfur, S <= 0.050 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI 1015 Steel, as rolled
AISI 1015 Steel, cold drawn
AISI 1015 Steel, normalized at 925°C (1700°F)
AISI 1010 Steel, hot rolled bar, 19-32 mm (0.75-1.25 in) round or thickness
AISI 1015 Steel, cold drawn, 19-32 mm (0.75-1.25 in) round

M1015C / 6792

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.