MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Hexcel® Redux® 322 Modified epoxy film adhesive (0.078 psf)
Categories: Polymer; Adhesive; Film; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Redux 322 is a high performance modified epoxy film adhesive curing at 350°F. It is suitable for bonding metal to metal and for sandwich structures, where operating temperatures are experienced up to 430°F for short periods, or 390°F for continuous operation. Redux 322 is a hot melt film which is free from solvents and consequently has a very low volatile content.

Features: Cure at 350°F; Good co-cure potential with 350°F curing prepregs; Good hot lap shear performance; Good high temperature performance in metal sandwich structures; Low volatile content and low out gassing properties; Available with or without a woven nylon carrier.
Applications: Metal to metal bonding; Sandwich constructions.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Outgassing - Total Mass Loss 0.41 %Recovered Mass Loss (RML), Typical result; ESA PSS-01-702
 1.74 %Total Mass Loss (TML), Typical result; ESA PSS-01-702
Collected Volatile Condensable Material 0.00 %ESA PSS-01-702
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 0.870 ksi
@Temperature 149 °C
Flatwise Tension
 1.16 ksi
@Temperature 21.1 °C
Flatwise Tension
Shear Strength 2.90 ksi
@Temperature 177 °C
Lap Shear
 3.19 ksi
@Temperature 21.1 °C
Lap Shear
 3.335 ksi
@Temperature 149 °C
Lap Shear
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 390 °F
 430 °F
 
Processing PropertiesOriginal ValueComments
Shelf Life 18.0 Month
@Temperature -17.8 °C
 
Descriptive Properties
Areal Weight (psf)0.078
Climbing Drum Peel (in-lb/3in)50.670°F
Roll Width (in)21
Standard Roll (ft2)430
SupportWoven nylon carrier

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Hexcel® Redux® 322 Modified epoxy film adhesive (0.05 psf)
3M 5180 General Purpose PTFE Skived Film Tapes
Westlake Plastics Imidex Thermoplastic Polyimide
Sandvik Kanthal PAC-240 Wire insulations and coatings
Resin Technology Group MX-2212 High Impact, Multi-Functional, UV Curing Adhesive

PHEXC447 / 99266

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.