MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Lanxess LEWATIT® MDS TP 220 Ion Exchange Resin
Categories: Polymer; Thermoset

Material Notes: Lewatit® MDS TP 220 is a macroporous, weakly basic resin with chelating bis-picolylamine groups attached to a styrene/divinylbenzene co-polymer. Its monodisperse bead size distribution combined with a small mean bead size results in improved adsorption kinetics and an approx. 25% higher copper binding capacity relative to Lewatit MonoPlus TP 220. Lewatit MDS TP 220 exhibits a very high osmotic and mechanical stability to meet the requirements of metal processing technologies. It is delivered in the protonated sulfate form and can therefore be used without pretreatment. Due to the smaller bead size a higher pressure sop factor has to be considered when dimensioning the vessel during process design. The increased sensitivity towards suspended solids requires efficient pre-filtration of the feed stream, e.g by convention sand filter or filter candles. At a pH of 2, heavy metal cations are removed from aqueous solution consistent with the following selectivity series: Cu2>>Ni2>>UO2>>Fe3>>Zn2>>Co2>>Cd2>>Fe2. Lewatit MDS TP 220 is especially suitable for the use in the following applications:
  • the purification of cobalt electrolytes (cobalt/nickel separation)
  • the separation of nickel/copper for ferric solutions
  • the recovery of copper from strongly acidic solutions (pH<2)
  • the purification of chromium (III) baths (removal of heavy metals such as copper and nickel)
  • the adsorption of heavy metals (e.g copper) from solutions containing strong chelating agents like EDTA
Whilst most metals are removed from the loaded resin with a conventional acid strip, copper can only efficiently be desorbed with ammonia solution.

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.725 g/cc0.0262 lb/in³
Density 1.13 g/cc0.0408 lb/in³
Bead Size 0.340 - 0.400 mm0.0134 - 0.0157 inMean
Storage Temperature -20.0 - 40.0 °C-4.00 - 104 °F
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 70.0 °C158 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 24.0 Month24.0 Month
 
Descriptive Properties
AppearanceOpaque
pH Operating Range1 - 14

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLANY8775 / 209167

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.