MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Unifrax Fiberfrax® Duraboard® 350ES Ceramic Fiber Board
Categories: Ceramic; Oxide; Aluminum Oxide; Silicon Oxide

Material Notes: Fiberfrax® Duraboard® products are a family of rigid, high-temperature ceramic fiber boards manufactured in a wet forming process using Fiberfrax alumina-silica fibers and binders. All Duraboard products offer low thermal conductivity, high temperature stability, uniform density, and excellent resistance to thermal shock and chemical attack.

This product uses a unique fiber formulation to obtain high strength and machinability not normally achieved in light-weight ceramic fiber board products. The innovative composite binder system using both inorganic and organic components results in a strength-to-weight ratio of more than three times that of standard refractory ceramic fiber boards. Improved physical characteristics of this product allows for easier handling and fabrication. Duraboard 350ES has more than three times the strength of standard boards of similar densities and thicknesses.

Description: Unique familiy of highly machinable lightweight boards manufactured with three to four times the green strength as standard board products.

Information Provided by Unifrax I LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.288 g/cc0.0104 lb/in³Nominal
Loss On Ignition 3.0 - 7.0 %3.0 - 7.0 %
 
Mechanical PropertiesMetricEnglishComments
Modulus of Rupture 0.000621 GPa0.0900 ksiFired (24 hrs at cont. use)
 0.00241 GPa0.350 ksiGreen (typ.)
Compressive Strength 0.186 MPa27.0 psi5% Deformation; Fired
 0.221 MPa32.0 psi10% Deformation; Fired
 0.228 MPa33.0 psi15% Deformation; Fired
 0.276 MPa40.0 psi5% Deformation; Green
 0.407 MPa59.0 psi10% Deformation; Green
 0.524 MPa76.0 psi15% Deformation; Green
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 1.06 kV/mm27.0 kV/in
 
Thermal PropertiesMetricEnglishComments
Melting Point 1760 °C3200 °F
Maximum Service Temperature, Air 1149 °C2100 °FRecommended Operating Temperature
Shrinkage <= 5.0 %
@Time 86400 sec
<= 5.0 %
@Time 24.0 hour
at Recommended Operating Temperature
 
Descriptive Properties
ColorWhite to Cream
Fiberfrax® Fibers (%)100
Temperature Grade (°C)1260

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Unifrax Fiberfrax® Durablanket® 2600 Ceramic Fiber Insulator
Unifrax Fiberfrax® Durablanket® S Ceramic Fiber Insulator
Unifrax Fiberfrax® Duraboard® 500ES Ceramic Fiber Board
Unifrax Fiberfrax® Fibermat® Blanket Ceramic Fiber Insulator
Unifrax Fiberfrax® Fibermax® Mat Ceramic Fiber Insulator

CUNIF029 / 97801

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.