MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Park Aerospace Nelcote® E-761 Epoxy Prepreg, Spectra® 951 - PT Reinforced
Categories: Polymer; Thermoset; Epoxy

Material Notes: Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.

Key Features and Benefits:

  • Controlled flow for ease of processing
  • Self adhesive for honeycomb or foam sandwich laminates without the use of film adhesive
  • Flexible cure temperature 180°F to 250°F
  • Good electrical properties
  • Flame and fire retardant per FAR 25.853
  • Wet service temperatures up to 160°F

Applications/Qualifications:

  • Radomes
  • Aircraft Interiors
  • Secondary Aircraft Structures
  • Sandwich Panels
  • MRI Resonators
  • Widely specified on commercial and military aircraft programs

Information provided by Park Electrochemical Corp.

Key Words: EP
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatiles <= 1.0 %
@Temperature 135 °C
8 min
Thickness 10.0 milPer Ply
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 65000 psi
@Temperature 21.1 °C
0° Direction, Dry; ASTM D638
Flexural Strength 14.0 ksi
@Temperature 21.1 °C
Dry; ASTM D790
Compressive Strength 5.00 ksi
@Temperature 21.1 °C
Dry; ASTM D695
Compressive Modulus 3900 ksi
@Temperature 21.1 °C
Dry; ASTM D695
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 2.6 - 2.8
@Frequency 5.00e+9 - 1.80e+10 Hz
Dissipation Factor 0.0040
@Frequency 5.00e+9 - 1.80e+10 Hz
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 115 °CDry; DMA
 
Processing PropertiesOriginal ValueComments
Gel Time 8.20 min
Shelf Life 12.0 Month
@Temperature -17.8 °C
 
Descriptive Properties
Fabric Area Weight (g/m²)98.3
Prepreg Resin Content (%)50
Resin Flow (%)6275°F, 50psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Hexcel® HexForce™ 328 Aramid Fabric
Park Aerospace Nelcote® E-761 Epoxy Prepreg, 4581 Quartz
DuPont Teijin Films Mylar® HP Polyester Film, 48 Gauge
Park Aerospace Nelcote® E-761 Epoxy Prepreg, 7781 E-Glass Reinforced
Park Aerospace Nelcote® E-761 Epoxy Prepreg, 6781 S2-Glass

PPARK026 / 89298

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.