MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Axiall ProTherm® 4526 CPVC Rigid PVC, Molding  (discontinued **)
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: Georgia Gulf ProTherm® 4526 CPVC is a pelletized injection molding compound designed for fittings. Typical applications are in potable water and chemical transfer systems especially where high resistance and/or elevated temperatures exist. 4526 has excellent processability, including thermal stability, flow, and surface appearance. ProTherm® 4526 is listed under NSF Standard 14 and Standard 61 and meets or exceeds ASTM D-1784 cell class 23447-B requirements.

Information provided by Georgia Gulf

Georgia Gulf became Axiall Corporation, which was later acquired by Westlake Plastics. This specific grade is discontinued.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.49 g/ccASTM D-792
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cmASTM D-955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 117ASTM D-785
Tensile Strength, Yield 8010 psiASTM D-638
Tensile Modulus 495000 psiASTM D-638
Flexural Strength 13000 psiASTM D-790
Flexural Modulus 405000 psiASTM D-790
Izod Impact, Notched 2.50 ft-lb/in
@Thickness 6.35 mm
ASTM D-256
Gardner Impact 180 in-lb
@Temperature 23.0 °C
1/2" R Tup, 180 mil
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 222.8 °Fannealed; ASTM D-648
Deflection Temperature at 1.8 MPa (264 psi) 213.8 °Fannealed; ASTM D-648
Vicat Softening Point 212 °F5kg Load at 50°C per Hour(annealed); ASTM D-1525A
Oxygen Index 44 %ASTM D-2863
 
Descriptive Properties
Cell Classification, ASTM D-178423447-B
Flow Ratio (Distance/Wall Thickness, 410-425°F)110Georgia Gulf Test

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Vycom Corzan® CPVC Chlorinated PVC
Axiall ProTherm® 4529 CPVC Rigid PVC, Molding
Overview of materials for PVC, Molded
Overview of materials for Chlorinated PVC (CPVC)
Vycom FLAMETEC™ CPVC Chlorinated Polyvinyl Chloride Sheet

PGGUL471 / 41747

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.