Garlock cloth-inserted materials are designed to add stability where mechanical fastening is necessary, and to reduce gasket creep where heavy flange loading is required. Style #2103 C.I. is a smooth-finish SBR/NBR sheet constructed with polyester fabric. Designed to reduce creep in flanges. Information provided by Garlock Rubber Technologies |