MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Dielectric Polymers NT-101PLT Double Liner Tape  (discontinued **)
Categories: Polymer; Adhesive; Tape; Thermoset

Material Notes: Acrylic adhesive with moisture stable PE coated kraft base release and high density PE interliner.

Features:

  • Clear releases liner allows easy inspection of back lighted panels
  • Plasticizer migration resistant
  • Chemical resistant

Applications:

Mounting nameplates, graphic panels and decorative trim. Bonding a wide variety of substrates.

Information provided by Dielectric Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 50.8 microns2.00 milAdhesive
 76.2 microns3.00 milInterliner
 
Mechanical PropertiesMetricEnglishComments
Peel Strength 0.614 kN/m3.50 pli180° peel, PET/s.s.
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 116 °C240 °FShear Adhesive Failure (cohesive failure)
 121 °C250 °FContinuous
 204 °C400 °FIntermittent
Minimum Service Temperature, Air -53.9 °C-65.0 °FContinuous

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDIEL29 / 30144

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.