MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Akrochem AKRO-MAG® BARS, BLUE LABEL MgO
Categories: Other Engineering Material

Material Notes: Product Description: AKRO-MAG BARS are a new form of Magnesium Oxide. The bar is a dispersion of naphthenic process oil with the highest activity magnesium oxide powder available having a typical Iodine absorption figure of 170 on the Morton Activity Index. The activity and particle size of the magnesia are the most important characteristics in determining the final properties of the vulcanized polychloroprene, Hypalon and Fluoroelastomers. The two Akrochem® MgO Bar Grades (Blue and Green) offer a choice of MgO activity and price. Blue offers the most active grade and thus the most scorch resistance in halogenated polymers like polychloroprene. Green bar offers a less active grade MgO that results in faster scorch and cures times

Information provided by Akrochem Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.49 g/cc
Specific Surface Area 170 m²/gAverage MgO
 
Descriptive Properties
AppearanceCream to Dark Tan
CarrierNaphthenic Oil
Content0.55Magnesium Oxide, MgO, Green Bar

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PAKZCH118 / 315036

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.