MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

BASF 2-Ethylhexanoic Acid
Categories: Fluid

Material Notes: Formula: C8H16O2

CAS: 149-57-5

Description: 2-Ethylhexanoic acid is a colorless to yellow liquid, with a faint specific odor. It is immiscible with water, but miscible with almost all conventional organic solvents.

Synonyms: 2-Butylbutanoic acid, 2-Ethylcaproic acid, 2-Ethylcapronsaure, Ethylhexanoic acid, Butylethylacetic acid 3-Heptanecarboxylic acid

Applications: Intermediate used in the production of Pharmaceuticals, Dyes and Polymers; Also used as a Additives for fuels and lubricants and Plasticize

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.910 g/cc0.0329 lb/in³
Molecular Weight 144.2 g/mol144.2 g/mol
 
Thermal PropertiesMetricEnglishComments
Melting Point -59.0 °C-74.2 °F
Boiling Point 226 - 229 °C439 - 444 °F
Flash Point 114 °C237 °F
Ignition Temperature 310 °C590 °F
 
Component Elements PropertiesMetricEnglishComments
H2O, Water <= 0.10 %<= 0.10 %DIN 51 777
 
Descriptive Properties
Assay>99.5%
Color<10APHA, DIN EN 1557

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBASG0938 / 132571

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.