MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Parson Adhesives PARFIX® 3412 Cyanoacrylate Adhesive
Categories: Polymer; Adhesive; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes: PARFIX 3412 is a very low viscosity with super-fast cure speed, surface insensitive cyanoacrylate adhesive. It is specifically formulated to bond difficult surfaces, wicking grade for close surface contact.

Applications:

  • Excellent adhesion to wide variety of Wood, Metal, Plastics, and Rubbers
  • High performance general purpose industrial applications

Information provided by Parson Adhesives, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Brookfield Viscosity 3.0 - 5.0 cP3.0 - 5.0 cPLVF, Spindle 1-60 rpm
 
Mechanical PropertiesMetricEnglishComments
Shear Strength 10.0 MPa1450 psiABS; ASTM D1002
 12.0 MPa1740 psiPolycarbonate; ASTM D1002
 18.0 MPa2610 psiEtched Aluminum; ASTM D1002
 20.0 MPa2900 psiGrit Blasted Steel; ASTM D1002
 22.0 MPa3190 psiRubbers; ASTM D1002
 18.0 - 28.0 MPa2610 - 4060 psi
 25.0 MPa3630 psiWood; ASTM D1002
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmASTM D257
Dielectric Constant 2.72.7ASTM D150
Dielectric Strength 0.984 kV/mm25.0 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
CTE, linear 75.0 µm/m-°C41.7 µin/in-°FASTM D696
Thermal Conductivity 0.100 W/m-K0.694 BTU-in/hr-ft²-°FASTM C177
Melting Point 160 - 170 °C320 - 338 °F
Maximum Service Temperature, Air 80.0 °C176 °F
Minimum Service Temperature, Air -51.1 °C-60.0 °F
Glass Transition Temp, Tg 120 °C248 °FASTM E228
 
Processing PropertiesMetricEnglishComments
Cure Time 1440 min24.0 hourFull
 
Descriptive Properties
AppearanceColorless liquid
CompositionSurface Insensitive Ethyl Cyanoacrylate
Gap Filling0.05 mm
Initial Strength Retained (%)75Gasoline for 1000 hrs at 22°C
 80Gasoline for 500 hrs at 22°C
 85Isopropanol for 500 hrs at 22°C
 85Isopropanol for 1000 hrs at 22°C
 90Motor Oil for 500 hrs at 40°C
 90Motor Oil for 1000 hrs at 40°C
 90Mineral Spirit for 500 hrs at 22°C
 90Mineral Spirit for 1000 hrs at 22°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
PTS Tristar® PC-20GFR 20% Glass Reinforced Polycarbonate With Release

PPARSN122 / 186565

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.