MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Nurel Engineering Polymers Promyde® B30 P2 G20 U0 PA 6, Conditioned, 20% Glass Reinforced, Injection Molded and Flame Retardant
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 20% Glass Fiber Filled

Material Notes: Characteristics: Promyde B30 P2 G20 U0 is a polyamide 6 with 20% glass fiber with high mechanical strength, heat stabilized, lubricated and nucleated for injection molding. Its halogen free flame retardant system enhances its flame behavior to V0- UL rated category.

Applications: Promyde B30 P2 G20 U0 allows a fast and efficient mould filling, and an easy mould release, that combined with its excellent mechanical properties, and its flame retardant properties make it suitable for components specially used in electrical and electronics industries.

Information provided by Nurel Engineering Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.36 g/cc0.0491 lb/in³ISO 1183
Moisture Absorption 2.30 %2.30 %50%, rh; ISO 62
Water Absorption at Saturation 6.9 %6.9 %in water; ISO 62
Viscosity Test 125 cm³/g1.25 dl/gViscosity Number; ISO 307
Linear Mold Shrinkage, Flow 0.0030 - 0.0035 cm/cm0.0030 - 0.0035 in/in
Linear Mold Shrinkage, Transverse 0.0040 - 0.0045 cm/cm0.0040 - 0.0045 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 40.0 MPa5800 psi50 mm/min; ISO 527-1/-2
Elongation at Break 5.0 %5.0 %50 mm/min; ISO 527-1/-2
Tensile Modulus 5.00 GPa725 ksi1 mm/min; ISO 527-1/-2
Flexural Strength 90.0 MPa13100 psi2 mm/min; ISO 178
Flexural Modulus 3.50 GPa508 ksi2 mm/min; ISO 178
Charpy Impact Unnotched 8.00 J/cm²
@Temperature 23.0 °C
38.1 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 2.50 J/cm²
@Temperature 23.0 °C
11.9 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+10 ohm-cm1.00e+10 ohm-cmIEC 60093
Surface Resistance 1.00e+10 ohm1.00e+10 ohmIEC 60093
Dielectric Constant 6.8
@Frequency 1e+6 Hz
6.8
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 V600 VIEC 60112
 
Processing PropertiesMetricEnglishComments
Mold Temperature 40.0 - 80.0 °C104 - 176 °F
Drying Temperature <= 80.0 °C<= 176 °F
Dry Time 4.00 - 6.00 hour4.00 - 6.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNUREL065 / 183430

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.