MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Kumho-Sunny HSG5415 SMA, 15% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; SMA Polymer; Glass Reinforced, Modified SMA

Material Notes: HSG5415 is an 15% glass fiber reinforced SMA alloy, offering high heat resistance, high modulus and low odor.

Application: Automobile interiors and exteriors such as instrument panel, console substrate, instrument panel ducts, etc.

Information provided by Shanghai Kumho Sunny Plastics co, Ltd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.17 g/ccISO 1183
Maximum Moisture Content 0.050
Linear Mold Shrinkage 0.0030 - 0.0050 cm/cmISO 294
Melt Flow 8.0 g/10 min
@Load 5.00 kg,
Temperature 265 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 115ISO 2039
Tensile Strength 73.0 MPa50mm/min; ISO 527
Elongation at Break 5.0 %50mm/min; ISO 527
Flexural Strength 110 MPa2mm/min; ISO 178
Flexural Modulus 5000 MPa2mm/min; ISO 178
Izod Impact, Notched (ISO) 10.0 kJ/m²5.5J; ISO 180
Charpy Impact Unnotched 30.0 kJ/m²4J; ISO 179
Charpy Impact, Notched 7.00 kJ/m²
@Thickness -30.0 mm
4J; ISO 179
 10.0 kJ/m²
@Thickness 23.0 mm
4J; ISO 179
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmIEC 60093
Surface Resistance >= 1.00e+15 ohmIEC 60093
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 117 °CASTM D648
Vicat Softening Point 120 °C
@Load 5.00 kg
50°C/h; ISO 306
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 220 - 230 °C
Middle Barrel Temperature 250 - 260 °C
Front Barrel Temperature 270 - 280 °C
Nozzle Temperature 270 - 280 °C
Melt Temperature 270 - 280 °C
Mold Temperature 70.0 - 90.0 °C
Drying Temperature 100 - 105 °C
Dry Time 4.00 - 6.00 hour
Back Pressure 1.00 - 5.00 MPa
Screw Speed 30 - 70 rpm
 
Descriptive Properties
Flammability15 mm/minISO3795

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PKMSN213 / 281065

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.