MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Petroquimica Triunfo Trithene® TS 7035 LDPE - Film - Lamination and Plastification  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: The Trithene TS 7035 resin is a low-density polyethylene (LDPE) with an excellent processability, which allows for a low energy consumption during extrusion and warrants the production of thin films with good appearance and optical properties, uniform thickness, strong heat sealing characteristics, and a good barrier to water vapor. The additive package warrants thermal stability, low blocking, and adequate coefficient of friction - COF, which are required to allow high productivity on the extrusion, printing and finishing lines. This product complies with ASTM standard D1248-IA3 and the requirements of Brazilian and corresponding legislation of Mercosul and it is in conformity with FDA Regulations 21 CFR 177.1520 (c) 2.1, to contact with foodstuff.

Applications: Composition of multi-material structure laminated films for packaging of miscellaneous products such as coffee, cookies, etc. Structure-plastified films or sheets. High transparent, very thin films.

Resin Properties: Compressed molded plate. Method ASTM D-1928, procedure C. Film obtained on a 50mm blow film line with barrier screw, 25:1 L/D, 1.0mm die gap, 50µm gauge, 2.3:1 BUR.

Information provided by Dax Resinas

Petroquimica Triunfo has been acquired by Braskem.

Key Words: FDA: 21 CFR 177.1520 (C) 2.1
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.922 - 0.925 g/ccASTM D1505
Thickness 50.0 microns
Melt Index of Compound 3.0 - 4.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 12.0 MPaASTM D638
Tensile Strength, Yield 10.0 MPaASTM D638
Film Elongation at Break, MD 410 %ASTM D882
Film Elongation at Break, TD 690 %ASTM D882
Elongation at Break 540 %ASTM D638
Secant Modulus, MD 0.0970 GPa5%; ASTM D882
Secant Modulus, TD 0.103 GPa5%; ASTM D882
Coefficient of Friction, Dynamic 0.090ASTM D1894
Elmendorf Tear Strength, MD 9.20 g/micronASTM D1922
Elmendorf Tear Strength, TD 6.20 g/micronASTM D1922
Dart Drop Test 125 g(method A); ASTM D1709
Film Tensile Strength at Break, MD 20.0 MPaASTM D882
Film Tensile Strength at Break, TD 18.0 MPaASTM D882
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 93.0 °CASTM D1525
 
Optical PropertiesOriginal ValueComments
Haze 8.2 %ASTM D1003
Gloss 100 %@ 60° Gardner; ASTM D2457
Transmission, Visible 90 %transparent; thickness not quantified
 
Processing PropertiesOriginal ValueComments
Processing Temperature 145 - 160 °CPlasticizing Zone
 150 - 165 °CMixture Zone
Feed Temperature 135 - 150 °C
Adapter Temperature 160 - 175 °C
Blow-up Ratio (BUR) 3.5Recommended
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mitsubishi Chemical Advanced Materials Proteus® LDPE - Low Density Polyethylene (ASTM Product Data Sheet)
Mitsubishi Chemical Advanced Materials Borotron® HD050 5% Boron-filled Polyethylene (ASTM Product Data Sheet)
Dow UNIVAL™ DMDF-6200 NT 7 High Density Polyethylene Resin (HDPE)
Total Finathene® 53140 HDPE, blow molding, sheet
Overview of materials for Low Density Polyethylene (LDPE), Sheet/Profile extrusions

PDAX089 / 29514

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.