MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Westlake Plastics

(Viewing data as-entered. Click here to return)
Westlake Plastics Propylux® SD-A Polypropylene (anti-static)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: Propylux® SD-A is a non-carbon-filled, permanently anti-static polypropylene (PP) offering surface resistivity in the 10EE9 to 10EE11 ohm/sq range. Propylux® SD-A is extremely low out-gassing, non-sloughing, and has been used in clean room environments. The material is available in both natural and black color.

Industry: Engineering; Semiconductor and ESD

Colors Available: Black, Natural

Attributes: Chemical Resistance; Impact Resistance

Shapes: Compression Sheet; Extruded Sheet

Information provided by Westlake Plastics Co.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.940 - 0.960 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 51.7 MPaASTM D638
Tensile Strength, Yield 13.8 MPaASTM D638
Elongation at Break >= 500 %ASTM D638
Elongation at Yield 24 %ASTM D638
Flexural Modulus 172.0 MPaASTM D790
Izod Impact, Notched NBASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+9 - 1.00e+11 ohm-cmASTM D257
Surface Resistance 1.00e+9 - 1.00e+11 ohmASTM D257
 
Descriptive Properties
ColorNatural - Off White, Camel, Black

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Westlake Plastics Propylux® SD-X7 Polypropylene (static dissipative)
Overview of materials for Polypropylene, Molded
Mitsubishi Chemical Advanced Materials Semitron™ ESd 480 PEEK, static dissipative
Westlake Plastics Propylux® Polypropylene
RTP Company RTP 1899 A X 106999 Polycarbonate/Acrylic Alloy (PC/PMMA), Permanently Anti-static - ESD Protection - Flame Retardant - Non-PBDE/PBB - UV Stabilized - UL94 V-0

PWEST042 / 72722

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.