MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ATI Allegheny Ludlum AL 444™ Ferritic Stainless Steel
Categories: Metal; Ferrous Metal; Ferritic; Stainless Steel; T S40000 Series Stainless Steel

Material Notes: Low carbon, low nitrogen ferritic stainless steel alloy.

Characteristics:practically immune to chloride stress corrosion cracking, enhanced resistance to pitting and crevicing, good general corrosion resistance, good creep resistance.

Applications: heat exchangers tubing, food processing equipment, automotive exhausts, and hot water tanks.

Information provided by Allegheny Ludlum

Key Words: UNS S44400
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.75 g/cc0.280 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 8080Typical
Tensile Strength, Ultimate 517 MPa75000 psiTypical
Tensile Strength, Yield 345 MPa
@Strain 0.2 %
50000 psi
@Strain 0.2 %
Typical
Elongation at Break 30 %30 %in 2", Typical
 
Thermal PropertiesMetricEnglishComments
CTE, linear 11.0 µm/m-°C
@Temperature 20.0 - 200 °C
6.11 µin/in-°F
@Temperature 68.0 - 392 °F
Specific Heat Capacity 0.427 J/g-°C0.102 BTU/lb-°F
Thermal Conductivity 26.8 W/m-K
@Temperature 100 °C
186 BTU-in/hr-ft²-°F
@Temperature 212 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.013 %0.013 %
Chromium, Cr 18.2 %18.2 %
Iron, Fe >= 79.79 %>= 79.79 %As Remainder
Manganese, Mn 0.30 %0.30 %
Molybdenum, Mo 1.9 %1.9 %
Nickel, Ni <= 0.50 %<= 0.50 %
Niobium, Nb (Columbium, Cb) 0.27 %0.27 %
Nitrogen, N 0.015 %0.015 %
Other 0.40 %0.40 %
Phosphorus, P <= 0.030 %<= 0.030 %
Silicon, Si 0.45 %0.45 %
Sulfur, S <= 0.0020 %<= 0.0020 %
Titanium, Ti 0.13 %0.13 %
 
Descriptive Properties
Corrosion Rate mils per year>100010% Sulfamic Acid, Boiling
 >100010% Sulfuric Acid, Boiling
 0.120% Acetic Acid, Boiling
 1.71% Hydrochloric Acid, Boiling
 10110% Oxalic Acid, Boiling
 1865% Nitric Acid, Boiling
 2.320% Phosphoric Acid, Boiling
 27.145% Formic Acid, Boiling
 29350% Sodium Hydroxide, Boiling
Pitting Potential, Volts vs. Sat. Calomel Electrode0.58
Stress Corrosion Cracking Resistance (ASTM G30)Pass42% MgCl2
 Pass33% LiCl
 Pass26% NaCl

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AK Steel 444 Ferritic Stainless steel
444 Ferritic Stainless Steel, 18Cr-2Mo (UNS S44400)
3M 444 Double Coated Tapes with Adhesive 300
316 Stainless Steel, annealed sheet
304 Stainless Steel

NL1019 / 17787

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.