MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Rogers Corporation RO3206 Woven-Glass Reinforced PTFE Laminate
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE); Polytetrafluoroethylene (PTFE), Glass Filled, Molded

Material Notes: Features and Benefits:
  • Woven glass reinforcement - Improves rigidity for easier handling
  • Uniform electrical and mechanical performance - ideal for complex multi-layer high frequency structures
  • Low dielectric loss - high frequency performance can be used in applications exceeding 20 GHz
  • Low in-plane expansion coefficient (match to copper) - suitable for use with epoxy multi-layer board hybrid designs and allows for more reliable surface mounted assemblies
  • Excellent dimensional stability - high production yields
  • Economically priced - cost effective volume manufacturing
  • Surface smoothness- allows for finer line etching tolerances
  • Lead-free process compatible

Uses:

  • Automotive collision avoidance systems
  • Automotive global positions satellite antennas
  • Wireless telecommunications systems
  • Microstrip patch antennas for wireless communications
  • Direct broadcast satellites
  • Datalink on cable systems
  • Remote meter readers
  • Power backplanes
  • LMDS and wireless broadband
  • Base station infrastructure

Information provided by Rogers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.70 g/cc
Water Absorption <= 0.10 %D24/23; IPC-TM-2.4.8
Thickness 25.0 - 50.0 milRange of Thicknesses Available
 
Mechanical PropertiesOriginal ValueComments
Tensile Modulus 462 ksiMD; ASTM D638
 462 ksiTD; ASTM D638
Peel Strength 10.7 pliCopper; 1 oz. EDC After Solder Float; IPC-TM-650 2.4.8
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+9 ohm-cmCond. A; IPC 2.5.17.1
Surface Resistance 1.00e+9 ohmCond. A; IPC 2.5.17.1
Dielectric Constant 6.0 - 6.3
@Frequency 1e+10 Hz
Clamped stripline, Z-direction; IPC-TM-650 2.5.5.5
 6.6
@Frequency 8.00e+9 - 4.00e+10 Hz
Differential Phase Length Method, Z-Direction
Dissipation Factor 0.0027
@Frequency 1e+10 Hz
IPC-TM-650 2.5.5.5
 
Thermal PropertiesOriginal ValueComments
CTE, linear 13.0 µm/m-°C
@Temperature -55.0 - 288 °C
X, Y- Direction; ASTM D3386-94
 34.0 µm/m-°C
@Temperature -55.0 - 288 °C
Z-Direction; ASTM D3386-94
Specific Heat Capacity 0.850 J/g-°CCalculated
Thermal Conductivity 0.670 W/m-K
@Temperature 80.0 °C
ASTM C518
Decomposition Temperature 500 °CTGA; ASTM D3850
Flammability, UL94 V-0
 
Descriptive Properties
Dimensional Stability0.8 mm/mASTM D257, Cond. A; X, Y-direction
Thermal Coefficient of Dielectric Constant-212 ppm/°CIPC-TM-650 2.5.5.5; 10 GHz; 0°C to 100°C; Z-Direction

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Techmer ES Plaslube® J-50/30/TF/15 Polycarbonate, 30% Glass Reinforced, PTFE Lubricated
Techmer ES Plaslube® J-50/20/TF/15 Polycarbonate, 20% Glass Reinforced, PTFE Lubricated
Saint-Gobain Chemfab® 3 Basic PTFE-Coated Glass
Saint-Gobain Chemfab® 14 Primary PTFE-Coated Glass
Rogers Corporation TMM® TMM6 Ceramic Thermoset Polymer Composite

PROGA951 / 138391

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.