MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
ITW Permatex® Penetrating Grade Threadlocker GREEN
Categories: Polymer; Adhesive; Thermoset

Material Notes: Permatex Penetrating Grade Thread locker GREEN is a medium strength anaerobic thread locking material, which cures between engaged threads to form a unitized assembly that helps resist leakage, shock and vibration. The product is a single component, anaerobic liquid that cures in the absence of air and when confined between close fitting metal surfaces. Because of its low viscosity and capillary action, the product wicks between engaged threads and eliminates the need to disassemble, apply product and then reassemble. The high prevailing torque provides vibration resistance to adjustment screws. Ideal for all threaded engagements less than or equal to 1/2 inch in diameter. The product can also fill porosity in welds, castings and powder metal parts. Excellent chemical resistance and temperature range of -54°C to +149°C (-65°F to +300°F). Meets or exceeds the requirements of Military Specification Mil-S-46163A Type III, Grade R. NSF White Book registered.

The rate of cure will depend on the material used. Permatex Penetrating Grade Threadlocker GREEN will react faster and stronger with Active Metals. However, Inactive Metals will require the use of an activator (Surface Prep) to obtain maximum strength and cure speed at room temperature. The rate of cure will depend on the ambient temperature. Full cure is attainable in 24 hours at room temperature, 22°C (72°F), or 1 hour at 93°C (200°F). Where cure speed is unacceptably long, or large gaps are present, applying an activator (Surface Prep) to the surface will improve cure speed. A 3/8-16 steel nut and bolt assembly will fixture in 3 minutes using an activator, while fixturing will occur in 20 minutes without an activator. Full cure in 24 hours for both procedures. The graph below shows the breakaway strength developed with time using Permatex Surface Prep Activator.

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.08 g/ccUncured
Brookfield Viscosity 20 - 55 cPUncured. Brookfield RVF, spindle #1, @ 50 RPM.
 
Thermal PropertiesOriginal ValueComments
Flash Point >= 200 °F
 
Descriptive Properties
Chemical TypeAnaerobic Dimethacrylate Ester
Chemical/Solvent Resistance (%)100Gasoline. 500 hr @ 23°C
 100Antifreeze. 500 hrs @ 87°C.
 100Ethanol. 500 hrs @ 23°C
 100Acetone. 500 hrs @ 23°C
 35Hot air. 1000hrs @ 150°C.
 60Motor Oil. 1000 hr @ 125°C.
ColorGreen Fluorescent LiquidUncured

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PITWP9136 / 239646

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.