PUROLAN® PE is a clear, colorless liquid. It can be used as a preservative and as a solvent. Consumer Products: For the preservation of cosmetic, toiletry and household products and their raw materials. Effective against Gram positive and Gram negative bacteria and fungi. It is often used together with other active substances. Surface & Instrument Disinfection: Used in combination with other active ingredients for the formulation of disinfectants for hard surfaces, disinfectant cleaners and surgical instruments.INCI: Phenoxyethanol CAS No.: 122-99-6 EINECS No.: 204-589-7 Information provided by Lanxess. |