MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

AISI 15B21H Carbon Steel, Composition Spec
Categories: Metal; Ferrous Metal; Carbon Steel

Material Notes: The B designation indicates added boron to increase the hardenability after quenching.

Key Words: UNS H15211; SAE 15B21H
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.85 g/cc0.284 lb/inĀ³Estimated by MatWeb from very similar grade
 
Component Elements PropertiesMetricEnglishComments
Boron, B 0.00050 - 0.0030 %0.00050 - 0.0030 %
Carbon, C 0.17 - 0.24 %0.17 - 0.24 %
Iron, Fe 98.17 - 98.9795 %98.17 - 98.9795 %As Balance
Manganese, Mn 0.70 - 1.2 %0.70 - 1.2 %
Phosphorus, P <= 0.040 %<= 0.040 %
Silicon, Si 0.15 - 0.30 %0.15 - 0.30 %
Sulfur, S <= 0.050 %<= 0.050 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI 15B35H Carbon Steel, Composition Spec
AISI 15B37H Carbon Steel, Composition Spec
AISI 1021 Steel, cold rolled, 25 mm (1 in.) round
AISI 50B40 Steel
AISI 1022 Steel, cold drawn round (19 - 32 mm)

M1521BH / 147575

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.