MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company RTP 899 X 120422 A Acetal (POM); Carbon Nanotube - ESD Protection - Static Dissipative
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM)

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.42 g/cc1.42 g/ccASTM D 792
Linear Mold Shrinkage 0.015 - 0.025 cm/cm
@Thickness 3.20 mm
0.015 - 0.025 in/in
@Thickness 0.126 in
ASTM D 955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 60.0 MPa8700 psiASTM D 638
Elongation at Break >= 8.0 %>= 8.0 %ASTM D 638
Tensile Modulus 2.34 GPa340 ksiASTM D 638
Flexural Strength 85.5 MPa12400 psiASTM D 790
Flexural Modulus 2.62 GPa380 ksiASTM D 790
Izod Impact, Notched 0.481 J/cm
@Thickness 3.20 mm
0.900 ft-lb/in
@Thickness 0.126 in
ASTM D 256
Izod Impact, Unnotched 4.81 J/cm
@Thickness 3.20 mm
9.00 ft-lb/in
@Thickness 0.126 in
ASTM D 4812
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 1000 ohm-cm<= 1000 ohm-cmASTM D 257
Surface Resistance <= 1.00e+6 ohm<= 1.00e+6 ohmESD STM11.11
Surface Resistivity per Square <= 1.00e+7 ohm<= 1.00e+7 ohmASTM D 257
Static Decay <= 0.50 sec<= 0.50 secFTMS101C; 4046.1
 
Processing PropertiesMetricEnglishComments
Melt Temperature 182 - 204 °C360 - 400 °F
Mold Temperature 71.1 - 93.3 °C160 - 200 °F
Drying Temperature 82.2 °C
@Time 7200 sec
180 °F
@Time 2.00 hour
Moisture Content 0.10 %0.10 %
Dew Point -31.7 °C-25.0 °F
Injection Pressure 68.9 - 103 MPa10000 - 15000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Kingfa MAC-601 DY Modified 60/40 PC/ABS Alloy
Celanese FORTRON 300 PPS, Unfilled
RTP Company RTP 727 High Density Polyethylene (HDPE), Talc
RTP Company RTP 200 AR 10 TFE 10 Nylon 6/6 (PA); Aramid Fiber - PTFE Lubricated
RTP Company ESD C 600 Acrylonitrile Butadiene Styrene (ABS), ESD Protection - Electrically Conductive

PQZUA13693 / 134662

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.