MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Plenco 1510 Polyester, Granular, Transfer Molded  (discontinued **)
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Polyester, TS; Thermoset Polyester, Mineral Filled

Material Notes: PLENCO 01510 is a mineral filled, pelletized polyester molding compound, which offers an excellent combination of electrical properties and dimensional stability. UL recognized under component file E40654. 01510 is available in black.

Information supplied by Plenco.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.900 g/cc0.0325 lb/in³ASTM D1895
Density 2.01 g/cc0.0726 lb/in³ASTM D792
Water Absorption 0.133 %0.133 %ASTM D570
Linear Mold Shrinkage 0.00153 cm/cm0.00153 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell E 7878ASTM D785
Tensile Strength, Ultimate 77.0 MPa11200 psiASTM D638
Elongation at Break 0.55 %0.55 %ASTM D638
Tensile Modulus 19.8 GPa2870 ksiASTM D638
Flexural Strength 119 MPa17300 psiASTM D790
Flexural Modulus 19.9 GPa2890 ksiASTM D790
Compressive Strength 194 MPa28100 psiASTM D695
Poissons Ratio 0.2840.284ASTM D638
Shear Modulus 7.71 GPa1120 ksiCalculated
Izod Impact, Notched 0.223 J/cm0.418 ft-lb/inASTM D256
Charpy Impact, Notched 0.274 J/cm²1.30 ft-lb/in²ASTM D256
Impact 123123J/m Drop Ball Impact; PLENCO
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.60e+15 ohm-cm2.60e+15 ohm-cmASTM D247
Dielectric Constant 4.74.7ASTM D150
Dielectric Strength 11.8 kV/mm300 kV/inStep by Step; ASTM D149
 15.5 kV/mm394 kV/inShort Time; ASTM D149
Dielectric Breakdown 23000 V23000 V1hr 120C; ASTM D149
Dissipation Factor 0.01490.0149ASTM D150
Arc Resistance 192 sec192 secASTM D495
Comparative Tracking Index 600 V600 VASTM D3638
 
Thermal PropertiesMetricEnglishComments
CTE, linear 54.0 µm/m-°C
@Temperature 40.0 - 130 °C
30.0 µin/in-°F
@Temperature 104 - 266 °F
TMA; ASTM E831
Thermal Conductivity 0.730 W/m-K
@Temperature 100 °C
5.07 BTU-in/hr-ft²-°F
@Temperature 212 °F
ASTM E1461
Maximum Service Temperature, Air 213 °C415 °FHeat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 251 °C484 °FASTM D648
Flammability, UL94 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
Oxygen Index 25.5 %25.5 %ASTM D2863
Shrinkage 0.0167 %0.0167 %72 hr, 120ºC; ASTM D1299

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Plenco 1501 Polyester, Briquette, Transfer Molded
Plenco 1500 Polyester, Granular, Transfer Molded
Plenco 1500 Polyester, Granular, Compression Molded
C-Glass Fiber, Generic
Plenco 1508 Polyester, Briquette, Transfer Molded

PLEL19 / 50587

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.