MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

(Viewing data as-entered. Click here to return)
Aluminum 710.0-T5, Sand Cast
Categories: Metal; Nonferrous Metal; Aluminum Alloy; Aluminum Casting Alloy

Material Notes: Data points with the AA note have been provided by the Aluminum Association, Inc. and are NOT FOR DESIGN.

Composition Notes:
Composition information provided by the Aluminum Association and is not for design.

Key Words: Aluminium 710.0-T5; UNS A07100; AA710.0-T5; Al710.0-T5
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.81 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 60 - 90AA; Typical; 500 g load; 10 mm ball
Hardness, Knoop 98Estimated from Brinell Hardness.
Hardness, Vickers 85Estimated from Brinell Hardness.
Tensile Strength, Ultimate >= 32.0 ksiAA
Tensile Strength, Yield >= 20.0 ksi
@Strain 0.2 %
AA
Elongation at Break >= 2.0 %AA; in 2 in. (50 mm) or 4D
Tensile Modulus 71.0 GPaAluminum 770.0
Poissons Ratio 0.33Estimated from aluminum 770.0
Machinability 90 %0-100 Scale (100=best)
Shear Modulus 26.5 GPaEstimated from aluminum 770.0
Shear Strength 135 MPaCalculated
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000490 ohm-cm
 
Thermal PropertiesOriginal ValueComments
Heat of Fusion 389 J/gTypical for cast aluminum
CTE, linear 24.1 µm/m-°C
@Temperature 20.0 - 100 °C
 26.3 µm/m-°C
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.963 J/g-°CTypical for cast aluminum
Thermal Conductivity 138 W/m-K
Melting Point 596 - 646 °C
Solidus 596 °C
Liquidus 646 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 90.5 - 93.1 %As remainder
Copper, Cu 0.35 - 0.60 %
Iron, Fe <= 0.50 %
Magnesium, Mg 0.60 - 0.80 %
Manganese, Mn <= 0.05 %
Other, each <= 0.05 %
Other, total <= 0.15 %
Silicon, Si <= 0.15 %
Titanium, Ti <= 0.25 %
Zinc, Zn 6.0 - 7.0 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aluminum 713.0-T5, Sand Cast
Aluminum 707.0-T7, Sand Cast
Aluminum 712.0-F, Sand Cast
Aluminum 712.0-T5, Sand Cast
Aluminum 514.0-F, Sand Cast

MAC7100T5 / 10174

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.