Product description: Grilamid TR 30 LS natural is a high purity transparent thermoplastic polyamide, based on aliphatic and cycloaliphatic monomers. Grilamid TR 30 LS natural contains a processing aid to improve the flow- and demolding properties. Grilamid TR 30 LS natural offers outstanding properties such as:- very high stiffness
- good impact performance
- excellent transparency
- high surface hardness and gloss
- good scratch resistance
- chemical resistance especially vs. oil, grease and fuels
- stress cracking resistance
Grilamid TR 30 LS natural is especially suited for production of optical and technically demanding parts in the application fields of:- Electrical / Electronics
- Engineering
- Pneumatics
- Automotive
Information provided by EMS Grivory. |