System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
CHT Group QSil 551 QSI Quantum Silicones Silicone Potting Material
(discontinued **)
Categories:
Polymer
;
Thermoset
;
Silicone
Material Notes:
Part of the Amber Chemical Group. Data provided by manufacturer.
Characteristics:
100% solid, long pot life, low modulus, good elongation.
Formerly Amber Chemical Co (ACC Silicones), aquired by CHT in 2017
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Specific Gravity
1.40
g/cc
"B" component
1.40
g/cc
"A" component
Viscosity
3000
cP
"B" component
4000
cP
"A" component
Mechanical Properties
Original Value
Comments
Hardness, Shore A
30
catalyzed
Tensile Strength
>=
1.70
MPa
catalyzed
Elongation at Break
>= 200 %
catalyzed
100% Modulus
>=
0.150
ksi
@Strain 100 %
catalyzed
Tear Strength
>=
15.0
pli
catalyzed
Electrical Properties
Original Value
Comments
Volume Resistivity
2.60e+14
ohm-cm
Dielectric Constant
2.9
@Frequency 1000 Hz
Dielectric Strength
444.5
V/mil
Thermal Properties
Original Value
Comments
Thermal Conductivity
0.370
W/m-K
Flammability, UL94
V-1
@Thickness 1.50 mm
V-0
@Thickness 3.00 mm
Processing Properties
Original Value
Comments
Pot Life
>=
120
min
Descriptive Properties
Color
Beige
"A" component
Black
"B" component
**
Materials flagged as discontinued (
) are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.
Users of our Advanced Search (registration required) may exclude discontinued materials from search results.
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
CHT Group QSil 430 QSI Quantum Silicones Silicone Potting Material
CHT Group QSil 550 QSI Quantum Silicones Silicone Potting Material
CHT Group QSil 553 QSI Quantum Silicones Silicone Potting Material
Overview of materials for Silicone Rubber
CHT Group QSil 550R QSI Quantum Silicones Silicone Potting Material
PACC033 / 22160
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.