MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Phillips 66 Cotton Picker NLGI Grade 00
Categories: Fluid; Lubricant; Lithium Gellant

Material Notes: Cotton Picker is a high-quality, semifluid lithium grease developed for the lubrication of cotton picker spindle heads on the front of mechanical cotton pickers. It is formulated to protect the spindle heads, as well as the rapidly rotating cotton plant strippers. Cotton Picker is manufactured with high-quality base oils and lithium 12-hydroxystearate soap thickener. It is fortified with rust and oxidation inhibitors to protect the spindle heads and bearings against corrosion. Its semifluid consistency helps ensure complete lubrication and ease of starting of machinery during the fall harvest season as temperatures begin to drop. It is dyed green for ease of identification.

Applications:

  • Cotton picker spindles, picker bars and chassis bearings
Cotton Picker is recommended for use where the OEM specifies:
  • John Deere JDN 305, JDN 360
  • International Harvester IH B-27
Features/Benefit:
  • Protects spindles and bearings
  • Eliminates spindles seizure or freeze-up
  • Permits easy starting in cold weather
  • Protects against rust and corrosion

Information provided by Phillips 66 Lubricants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.884 g/cc0.0319 lb/in³
Viscosity Measurement 8080Index
Saybolt Viscosity at 100°F 118 SUS118 SUS
Saybolt Viscosity at 210°F 40.4 SUS40.4 SUS
Kinematic Viscosity at 40°C (104°F) 22.5 cSt22.5 cSt
Kinematic Viscosity at 100°C (212°F) 4.2 cSt4.2 cSt
Oxidative Stability 100 hour
@Pressure 0.0345 MPa
100 hour
@Pressure 5.00 psi
Pressure Drop; ASTM D942
 
Mechanical PropertiesMetricEnglishComments
Four Ball Wear 0.600 mm0.0236 inScar Diameter; ASTM D2266
Penetration 400 - 430400 - 430Unworked; ASTM D217
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 93.0 °C199 °F
Minimum Service Temperature, Air -29.0 °C-20.2 °F
 
Descriptive Properties
ColorDark Green
ThickenerLithium

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WCON5109 / 198362

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.