MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BASF Ultramid® A3X4G7 35% Glass Filled PA66 FR (Dry)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 40% Glass Fiber Filled

Material Notes: Description: 35% glass-fiber reinforced injection-molding grade with improved flame retardance and enhanced long-term stability. Flame retardant based on red phosphorus; very high stiffness and strength; outstanding mechanical and electrical properties.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.46 g/ccISO 1183
Viscosity Measurement 150ISO 307
Linear Mold Shrinkage 0.0040 cm/cmrestricted
Melt Flow 21.9 g/10 min
@Load 5.00 kg,
Temperature 275 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 130 MPa50 mm/min; ISO 527-1/-2
Elongation at Yield 2.3 %50 mm/min; ISO 527-1/-2
Modulus of Elasticity 9.80 GPaISO 527-1/-2
Charpy Impact Unnotched 60.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index 600 VTest solution A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
Melting Point 260 °CDIN 53765
Deflection Temperature at 1.8 MPa (264 psi) 250 °CISO 75-1/-2
Flammability, UL94 V-1
@Thickness >=0.400 mm
 
Processing PropertiesOriginal ValueComments
Melt Temperature 280 - 300 °CInjection-molding/Extrusion
Mold Temperature 80.0 - 90.0 °CInjection-molding
 
Descriptive Properties
Commercial StatusEurope

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultramid® A3HG6 Balance 30% Glass Filled PA 66/610 (Conditioned)
Domo Technyl® A20V25 25% Glass Filled, V-0 Nylon 66
Celanese Zytel® FR50 NC010 PA66-GF25FR(17)
Overview of materials for Nylon 66, Unreinforced
Mitsubishi Chemical Advanced Materials TIVAR™ 1000 Virgin UHMW-PE, (Natural & Colors except Black)

PBASG0314 / 131947

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.